详细介绍: 阻燃树脂 高耐热性 ABS AF-312B 广州LG Testing |
属性名称 |
测试方法 |
测试条件 |
Unit |
代表值 |
|
Flammability |
Flammability |
UL94 |
1/10" |
class
|
V-0, 5VB
|
Flammability |
UL94 |
1/16" |
Class
|
V-0
|
Flammability |
UL94 |
1/8" |
class
|
V-0, 5VB
|
Mechanical |
IZOD Impact strength |
ASTM D256 |
1/4″,23℃ |
kg·cm/cm
|
23
|
Elongation at Break |
ASTM D638 |
50mm/min |
%
|
20
|
IZOD Impact strength |
ASTM D256 |
1/8″,23℃ |
kg·cm/cm
|
30
|
IZOD Impact strength |
ASTM D256 |
1/8″,-30℃ |
kg·cm/cm
|
8
|
Tensile Strength at Yield |
ASTM D638 |
50mm/min |
kg/㎠
|
450
|
Flexural Strength |
ASTM D790 |
15mm/min |
kg/㎠
|
720
|
Tensile Modulus |
ASTM D638 |
50mm/min |
kg/㎠
|
23,000
|
Flexural Modulus |
ASTM D790 |
15 mm/min |
kg/㎠
|
26,000
|
IZOD Impact strength |
ASTM D256 |
1/4″,-30℃ |
kg·cm/cm
|
8
|
Elongation at Yield |
ASTM D638 |
50mm/min |
%
|
5
|
Physical |
Melt Index |
ASTM D1238 |
230℃/3.8kg |
g/10min
|
15
|
Mold Shrinkage |
ASTM D955 |
- |
%
|
0.4~0.7
|
Specific Gravity |
ASTM D792 |
23℃ |
|
1.19
|
Melt Index |
ASTM D1238 |
220℃/10kg |
g/10min
|
50
|
Melt Index |
ASTM D1238 |
200℃/5kg |
g/10min
|
6
|
Thermal |
Heat Deflection Temp |
ASTM D648 |
1/4″,4.6kg/㎠(annealed) |
˚C
|
87
|
Heat Deflection Temp |
ASTM D648 |
1/4″,4.6kg/㎠(unannealed) |
˚C
|
83
|
Heat Deflection Temp |
ASTM D648 |
1/4″,18.5kg/㎠(unannealed) |
˚C
|
75
|
Heat Deflection Temp |
ASTM D648 |
1/4″,18.5kg/㎠(annealed) |
˚C
|
82
|
Vicat Softening Temp |
ASTM D1525 |
5kg, 50℃/hr |
˚C
|
83
|
|
|